Conductive thin coating made of AgNWs

From Hackteria Wiki
Revision as of 11:52, 2 October 2023 by Shihweichieh (talk | contribs) (Created page with "==Preparation of AgNWs solutions== The dispersion of AgNWs was spin-coated (500 rpm for 20 s) onto the glass and heated on a hot plate at 60 °C for 5 min to remove any remain...")
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)
Jump to: navigation, search

Preparation of AgNWs solutions

The dispersion of AgNWs was spin-coated (500 rpm for 20 s) onto the glass and heated on a hot plate at 60 °C for 5 min to remove any remaining organic solvent.