abstract

Conventionally it requires 450 to 500 celsius to sinter the TiO2 porous layer which functioning as the photo-electrode in dye sensitized solar cell, it eliminates the application of flexible DSSC manufactured in textile or plastic substrates. There are two possible solutions to make the TiO2 porous layer in flexible DSSC device: 1. sintering the TiO2 porous layer on textile or plastic film with temperature lower than 150 celsius or in room temperature. 2. sintering the TiO2 layer on high heat resistive textile substrates. Here the first option is being experimented.